Intermediate Annealing at 450 °C Cuts Resistance of Spray-Pyrolyzed Bilayer ZnO Films
Spray-pyrolyzed undoped bilayer ZnO films intermediate-annealed at 450 °C showed a sheet resistance of 54.1 Ω/□ and the study's highest ...
Spray-pyrolyzed undoped bilayer ZnO films intermediate-annealed at 450 °C showed a sheet resistance of 54.1 Ω/□ and the study's highest ...