Surface topography fundamentally governs how contacting metallic components interact, dissipate frictional energy, and degrade under dynamic mechanical loads. In a comprehensive investigation evaluating aerospace structural materials, researchers systematically examined the influence of initial surface roughness on the wear behavior of TC11 titanium alloy through coupled reciprocating friction experiments and finite element simulations. TC11 titanium alloy, defined by its nominal chemical composition of titanium, 6.5 percent aluminum, 3.5 percent molybdenum, 1.5 percent zirconium, and 0.3 percent silicon, possesses high mechanical strength, low density, and outstanding thermal stability. Because of these favorable physical characteristics, the alloy is widely utilized in the manufacturing of critical aircraft load-bearing structures and aero-engine components, most notably compressor blades and blisks. During normal aero-engine operation, structural connection interfaces are continuously subjected to severe vibrational loading and centrifugal forces. These operating forces induce interface wear, which degrades operational safety, curtails the service lifespan of engine blades, and alters structural mating clearances. Investigating how microscale roughness dictates interface degradation provides essential theoretical guidance for designing wear-resistant contact surfaces in critical turbomachinery assemblies.
Actual engineering contact surfaces are never perfectly smooth; instead, they are covered with randomly distributed microscopic asperities that dictate real contact area and local stress concentrations. To evaluate how representative surface finishes alter tribological performance, the experimental program tested TC11 specimens prepared with three distinct surface roughness values: 0.2 micrometers representing a high-precision finish, 0.4 micrometers representing a standard baseline finish, and 0.8 micrometers representing an upper operational limit. These specific values align directly with manufacturing standards for aero-engine connection structures, where surface roughness is typically held between 0.4 and 1.6 micrometers and refined to between 0.1 and 0.4 micrometers via precision polishing, while milling operations on integral impellers commonly yield roughness values ranging between 0.4 and 0.8 micrometers. Upper counter-specimens measuring 5 by 5 by 10 millimeters and lower test specimens measuring 10 by 15 by 5 millimeters were fabricated using low-speed wire electrical discharge machining with a machining precision of 0.1 micrometers, providing a nominal contact area of 5 by 5 millimeters. Precision grinding was subsequently applied to achieve the target roughness levels, verified by measuring five random square sampling zones of 0.64 by 0.64 millimeters on each contact surface.
Laboratory wear evaluations were conducted using a dry linear reciprocating test configuration at an ambient room temperature of 20 degrees Celsius. The experimental parameters were selected to reproduce the operating conditions encountered at aero-engine connection interfaces, incorporating a reciprocating stroke length of 2 millimeters, an operating frequency of 20 Hz, and a test duration spanning 24,000 cycles. To examine the interactive effects of mechanical pressure and topography, testing across each of the three roughness levels was carried out under three normal loads of 1.0 kN, 1.25 kN, and 1.5 kN, producing nine distinct operational test combinations. Throughout each reciprocating test, the real-time friction coefficient was recorded continuously as a function of cycle count. Following physical testing, post-test wear volume and maximum wear depth were quantified using a laser scanning confocal microscope. Specific volumetric wear rates were determined by normalizing total wear volume by the product of the applied normal load and the cumulative sliding distance, while worn surface morphologies and chemical compositions were analyzed using field emission scanning electron microscopy and energy-dispersive spectroscopy.
Friction coefficient measurements revealed that surface roughness dramatically alters the running-in behavior and stability of sliding interfaces. Under all evaluated test conditions, friction curves initially displayed a rapid increase during the running-in stage before leveling off into a steady-state wear regime. However, increasing the initial surface roughness substantially delayed the transition to the stable wear stage. For test specimens possessing a fine initial roughness of 0.2 micrometers, steady-state wear was achieved rapidly within 500 to 2,000 reciprocating cycles. When the surface roughness was increased to 0.4 micrometers, entering the stable wear regime required between 6,000 and 8,000 cycles. For the coarsest specimens with a surface roughness of 0.8 micrometers, running-in was severely prolonged, with the stable regime established only after approximately 18,000 cycles. Furthermore, the average friction coefficient recorded during the stable stage increased progressively alongside initial roughness, reflecting fundamental changes in the microscopic contact mechanics of tall asperities that experience intense local contact stresses, promote extensive plastic deformation, and generate large wear debris that resists running-in smoothing.
The experimental measurements also highlighted notable interactions between normal load and friction stability. Across tested specimens, increasing the applied normal load produced a gradual reduction in the steady-state friction coefficient. Under conditions combining low surface roughness with high normal loads, the friction coefficient exhibited minimal fluctuations and showed a slight declining trend over extended cycling. Conversely, interfaces combining high initial surface roughness with low normal loads maintained nearly constant average friction values over cycle progression but displayed much larger instantaneous fluctuations. This behavioral dichotomy stems directly from the mechanical behavior of wear debris generated between contacting bodies. Under substantial compressive normal loads, loose particulate debris is gradually compacted into an agglomerated layer, stabilizing sliding and reducing frictional resistance. On surfaces possessing elevated roughness, however, asperity fracture produces substantially larger debris fragments, while lower normal loads provide insufficient contact pressure to compact the particles effectively. The uncompacted debris particles remain free to plow through the metal interface, causing persistent frictional instability and amplified curve fluctuations.
Confocal microscopy measurements demonstrated that both maximum wear depth and specific wear rate increased significantly as initial surface roughness and normal load increased. Under identical normal loads, higher roughness consistently yielded deeper wear scars and accelerated material loss rates. Similarly, under a fixed roughness level, elevating the normal load amplified both wear depth and wear rate, with this upward trend becoming markedly more pronounced on rougher surfaces. These trends originate from severe microscopic stress concentrations: because rough surfaces make contact exclusively at isolated asperity summits, their actual contact area is vastly smaller than the nominal geometric contact area, creating localized stresses far exceeding bulk nominal pressures. Rougher surfaces generate sharper contact points and more acute stress peaks that accelerate elastoplastic damage. Post-test surface profilometry confirmed extensive morphological alteration across all specimens, revealing that wear processes increased contact surface roughness by a factor of 7.5 to 11 times relative to pre-test baseline values.
Scanning electron microscopy demonstrated that shifting initial roughness and normal load produces a pronounced transition in the underlying wear mechanisms. Under a light load of 1.0 kN, specimens with 0.2 micrometer roughness displayed relatively smooth surfaces marked by shallow plowing grooves and fine, scattered debris particles that partially consolidated into compacted patches. At 0.4 micrometers, plowing grooves deepened and wear pits emerged alongside localized debris agglomerations. At 0.8 micrometers under 1.0 kN, plowing grooves became deeper and wide debris clusters formed without establishing a coherent compacted layer, indicating that abrasive wear predominated. When the normal load was raised to 1.25 kN and 1.5 kN, the proportion of adhesive wear increased substantially across all specimens while abrasive wear diminished. At 1.5 kN, the 0.2 micrometer surfaces exhibited broader plowing grooves, extensive compacted debris layers, and emergent adhesive wear patches, whereas the 0.8 micrometer specimens developed extensive adhesive wear regions alongside a marked decrease in loose debris.
The shift toward adhesive wear at higher roughness and load levels is driven by local contact pressure, thermal effects, and oxide film degradation. Taller asperities with smaller tip radii of curvature generate intense local contact pressures that readily exceed material shear thresholds, promoting localized cold welding between counter-surfaces. These severe contact stresses easily fracture protective surface oxide films, exposing reactive, high-surface-energy virgin titanium alloy that readily adheres to the opposing mating face. In addition, rougher contact interfaces generate greater frictional heating and higher localized temperature rises during reciprocating motion, further lowering resistance to plastic shearing and accelerating adhesion. Concurrently, deep micro-valleys on rougher surfaces trap loose abrasive debris, diminishing three-body abrasive plowing. Energy-dispersive spectroscopy revealed that wear debris comprised titanium and aluminum with minor amounts of molybdenum, zirconium, and silicon, with titanium exceeding 50 atomic percent. Oxygen content in the debris climbed from 8.94 percent to 40.87 percent as roughness and load increased, showing that frictional oxidation—producing titanium and aluminum oxides—intensified significantly, with initial surface roughness exerting a stronger influence on oxidation than load.
To simulate rough surface contacts numerically, researchers generated virtual three-dimensional rough surface profiles using MATLAB based on two distinct mathematical models: the midpoint displacement method and the Weierstrass-Mandelbrot fractal function. Fractal parameters were extracted from measured physical specimen profiles using the structure function method, which calculates the fractal dimension and characteristic scale coefficient by evaluating height differences across displacement increments. The midpoint displacement method employs fractional Brownian motion via an iterative Diamond-Square algorithm, introducing random Gaussian displacements at each subdivision step. In contrast, the Weierstrass-Mandelbrot function constructs surfaces by superimposing multi-frequency trigonometric terms scaled by continuous spectral parameters. Point cloud files generated from both algorithms were calibrated using arithmetic average surface roughness formulas, imported into SolidWorks to construct solid geometric models of the rough contact pairs, and coupled with an energy-based wear model in finite element software, wherein cumulative wear volume is proportional to frictional dissipated energy based on the ratio of Archard wear coefficients to steady-state friction coefficients.
Topographical comparisons showed that the two fractal generation methods yield starkly different surface characteristics. Profiles generated by the midpoint displacement method exhibited sharp localized peaks and moderate surface continuity due to the statistical independence of high-frequency random additions. Conversely, surfaces synthesized via the Weierstrass-Mandelbrot function displayed smoother asperity peaks and superior spatial continuity resulting from harmonic phase coupling across frequencies. When compared against actual laboratory surface profiles, both fractal models exhibited lower peak-to-valley values and reduced fluctuation amplitudes because simplified point cloud densities were utilized to ensure computational tractability in subsequent finite element meshes. Nevertheless, the Weierstrass-Mandelbrot surfaces captured true physical topographies with greater fidelity than midpoint displacement profiles. Stress analysis under a 1.25 kN load revealed that ideally smooth models produced artificially uniform stress distributions concentrated only at specimen edges, whereas midpoint displacement models generated moderately elevated stresses, and Weierstrass-Mandelbrot models produced pronounced, realistic stress concentrations localized at contacting asperity tips.
Wear depth simulations demonstrated that combining an energy wear model with Weierstrass-Mandelbrot fractal surfaces delivers superior predictive accuracy compared to traditional methods. When simulations relied solely on an empirical wear coefficient applied across an ideally smooth geometry, calculated wear depths exhibited massive prediction errors because the model failed to reproduce asperity stress concentrations. While midpoint displacement models improved upon smooth representations, their simplified topography still underpredicted wear severity. In contrast, finite element simulations incorporating Weierstrass-Mandelbrot fractal geometries matched experimental wear depth trends across all evaluated loads and roughness values. When evaluated across normal loads of 1.0 kN, 1.25 kN, and 1.5 kN, the wear depth prediction error for Weierstrass-Mandelbrot models was confined between 5.13 percent and 7.36 percent for 0.2 micrometer surfaces, between 9.36 percent and 12.63 percent for 0.4 micrometer surfaces, and between 11.69 percent and 13.96 percent for 0.8 micrometer surfaces.
The study also evaluated the temporal evolution of wear depth and identified key physical factors responsible for the remaining simulation errors. Both experimental observations and Weierstrass-Mandelbrot simulations under a 1.25 kN load demonstrated a clear two-stage wear process: an initial running-in stage characterized by rapid, decelerating wear depth accumulation, followed by a steady-state wear stage exhibiting linear depth growth over cycle progression. Higher initial roughness prolonged the running-in duration and produced slightly steeper growth slopes during the stable stage. Remaining numerical discrepancies arise primarily because finite element wear modeling applies continuous adaptive mesh updating without simulating the physical creation, motion, or plowing of discrete wear debris particles, which in physical experiments accumulate unevenly, amplify local contact stresses, and accelerate run-in wear. Furthermore, the energy wear formulation assumes uniform nodal contact pressure and a constant friction coefficient averaged from steady-state data, whereas real interfaces experience dynamic local pressure variations. Future research will focus on extending the predictive framework beyond dry room-temperature conditions to incorporate environmental temperature variations, fluid lubrication, and discrete wear debris mechanics.
Subject of Research: The influence of initial surface roughness and fractal topography modeling on the reciprocating wear behavior of TC11 titanium alloy
Article Title: Fractal-based analysis of the influence of TC11 surface roughness on wear behavior
Article References: Cheng, Z., Zhang, H., & Cui, H. (2026). Fractal-based analysis of the influence of TC11 surface roughness on wear behavior. Surface Science and Technology, 4(1), Article 42. https://doi.org/10.1007/s44251-026-00144-6
Image Credits: AI Generated
DOI: 10.1007/s44251-026-00144-6
Keywords: TC11 titanium alloy, surface roughness, fractal modeling, Weierstrass-Mandelbrot function, midpoint displacement method, energy wear model, reciprocating wear, adhesive wear, abrasive wear, finite element simulation, tribology, wear debris, aero-engine components, contact stress, laser scanning confocal microscopy, scanning electron microscopy, energy-dispersive spectroscopy
News Source: Neil Sanderson. (November 24, 2026). Fractal Models Reveal How Surface Roughness Accelerates Titanium Alloy Wear. Scienmag.