Extruding a high-aluminum magnesium alloy significantly suppresses parasitic self-corrosion while maintaining strong electrochemical activation during discharge in saline environments, according to a laboratory investigation of primary magnesium–air battery anodes. The researchers evaluated how thermo-mechanical processing modifies internal phase architectures to address the longstanding trade-off between electrical output and unwanted material degradation in aqueous sodium chloride electrolytes.
Magnesium–air systems offer substantial promise for energy storage, yet their practical operational lifetime is frequently compromised by micro-galvanic corrosion and hydrogen gas evolution. To examine how composition and metallurgical processing influence these degradation mechanisms, the research team synthesized Mg–0.25Mn–xAl alloys with contrasting aluminum concentrations. They evaluated both low-aluminum and high-aluminum formulations in their initial as-cast conditions, designated as AM20 and AM90, alongside their thermo-mechanically extruded counterparts, designated as EXAM20 and EXAM90.
In the initial as-cast condition, augmenting the aluminum content altered the solid-state structure by refining the primary alpha-magnesium grains. However, in the high-aluminum cast formulation AM90, this compositional increase also precipitated a continuous network composed of aluminum-rich intermetallic beta-Mg17Al12 phases. While this continuous network facilitated initial discharge activation, it simultaneously accelerated localized micro-galvanic reactions across the matrix, driving severe parasitic self-corrosion and pronounced hydrogen gas evolution during electrolyte exposure.
To overcome this performance penalty, the investigators subjected the cast materials to a two-step metallurgical treatment consisting of thermal homogenization followed by hot extrusion. This thermo-mechanical sequence successfully fragmented and redistributed the continuous intermetallic network. The resulting microstructures exhibited fine recrystallized alpha-magnesium grains containing evenly dispersed aluminum-rich and aluminum–manganese-rich particulate phases rather than interconnected boundary pathways.
The electrochemical consequences of this structural redistribution were evaluated through immersion testing alongside time-dependent potentiodynamic polarization and electrochemical impedance spectroscopy in a 3.5 weight percent sodium chloride solution. Among all tested specimens, the extruded high-aluminum alloy EXAM90 achieved both the lowest overall immersion corrosion rate and the lowest volume of generated hydrogen gas under passive conditions.
During galvanostatic discharge assessments conducted over twenty-four hours at an applied current density of 10 milliamperes per square centimeter, EXAM90 sustained the most negative average discharge potential at negative 1.484 volts relative to a saturated calomel electrode. This steady operational potential confirmed that breaking apart the intermetallic network preserved favorable electrochemical activity without triggering the extensive corrosion typical of unworked high-aluminum magnesium castings.
The alloy also recorded an anodic efficiency of 51.0 plus or minus 1.2 percent, establishing the highest material utilization metric observed across the comparative cohort. In contrast to lower-efficiency variants where substantial active magnesium dissolves parasitically without generating external current, the extruded high-aluminum material directed a greater proportion of the consumed metal toward functional electrical output during prolonged discharge.
Microscopic analysis of the post-discharge surfaces demonstrated marked differences in the accumulation and shedding of reaction byproducts. Whereas the low-aluminum alloys retained persistent, passive magnesium hydroxide deposits that hindered electrolyte transport, EXAM90 formed discontinuous surface coverage with open channels. This porous morphology facilitated controlled byproduct detachment, preventing premature anode passivation.
These findings illustrate that processing-induced phase redistribution can decouple electrochemical activation from parasitic self-corrosion in magnesium-based battery anodes. By preventing continuous intermetallic pathways while maintaining fine particulate dispersion, this processing pathway presents a viable engineering strategy for primary magnesium–air batteries in marine instrumentation and emergency backup power supplies where extended operational endurance and efficient magnesium consumption are critical.
Subject of Research: Magnesium–air battery anode phase architecture and corrosion performance
Article Title: Processing-induced phase redistribution for enhanced self-corrosion control and discharge performance in Mg–Al–Mn anodes for Mg–air batteries
Article References: Najafi, M., Kashani-Bozorg, S. F., & Emamy, M. (2026). Processing-induced phase redistribution for enhanced self-corrosion control and discharge performance in Mg–Al–Mn anodes for Mg–air batteries. Materials for Renewable and Sustainable Energy. https://doi.org/10.1007/s40243-026-00391-5
Image Credits: AI Generated
DOI: 10.1007/s40243-026-00391-5
Keywords: magnesium-air batteries, anode materials, extrusion, phase redistribution, self-corrosion, anodic efficiency, discharge performance, Mg-Al-Mn alloys, intermetallic phases, hydrogen evolution, sodium chloride electrolyte, galvanostatic discharge, electrochemical impedance spectroscopy, potentiodynamic polarization, corrosion control, magnesium utilization, grain refinement, marine power systems
News Source: Faith Mcneil. (November 20, 2026). Extruded Magnesium Alloy Anode Cuts Self-Corrosion and Boosts Battery Utilization. Scienmag.