Autoclave sterilization did not significantly alter the maximum pull-out force of dental fiber posts subjected to different surface treatments in a controlled laboratory study. Researchers evaluated whether subjecting fiber posts to high-temperature steam sterilization before applying chemical or laser surface conditioning influenced post retention. Across all evaluated treatment combinations, the maximum force required to dislodge the cemented posts remained statistically indistinguishable between autoclaved and non-autoclaved specimens.
Fiber posts are routinely utilized in restorative dentistry to retain core restorations, with overall clinical retention depending partly on establishing effective bonding across the post, luting cement, and root dentin interfaces. Surface treatments such as chemical etching or laser conditioning are applied to enhance the mechanical and chemical adhesion between the fiber post and resin cement. However, dental practitioners face uncertainty regarding whether pre-treatment autoclave sterilization alters post surface properties or compromises retention.
To investigate these retention characteristics, investigators conducted an in vitro experiment utilizing sixty single-rooted human premolar teeth extracted due to periodontal disease. Following extraction, the crowns of the premolars were decoronated so that each test specimen consisted of a single root and one matching fiber post. The root specimens were nonrandomly allocated based on their root dimensions into four distinct experimental groups of fifteen specimens each within a two-by-two factorial design.
The experimental protocol tested two primary surface conditioning methods alongside the presence or absence of prior autoclave processing. Thirty fiber posts were processed in an autoclave at 134 degrees Celsius and 2 bar of pressure for 15 minutes prior to surface conditioning. For surface treatment, investigators conditioned the posts using either Er, Cr: YSGG laser irradiation or 37 percent phosphoric acid conditioning, creating four distinct cohorts: non-autoclaved acid-treated, autoclaved acid-treated, non-autoclaved laser-treated, and autoclaved laser-treated posts.
Following standard root canal treatment, technicians prepared 10-millimeter post spaces within the root canals of all decoronated specimens. Each conditioned fiber post was silanized and subsequently cemented into the prepared root canal space using a self-adhesive resin cement. To simulate storage aging, the assembled specimens were kept immersed in distilled water maintained at 37 degrees Celsius for six weeks prior to mechanical pull-out testing.
Mechanical testing was executed using a universal testing machine operating at a crosshead speed of 1 millimeter per minute. The testing machine recorded the maximum pull-out force measured in newtons and the displacement at maximum force measured in millimeters, defined specifically as the crosshead movement reached when peak force occurred. Stereomicroscopic inspection at 40-times magnification classified failure modes into cement–dentin adhesive failures, cement–post adhesive failures, or mixed failures.
Two-way analysis of variance demonstrated no significant main effects of autoclave sterilization, surface treatment, or their interaction on the maximum pull-out force, with all corresponding p-values exceeding 0.05. Conversely, displacement at maximum force exhibited a statistically significant interaction between autoclaving and surface conditioning, yielding an F-statistic of 8.389, a p-value of 0.005, and a partial eta squared of 0.130.
Further subgroup analysis revealed that autoclaved posts displayed significantly lower displacement than non-autoclaved posts when conditioned with 37 percent phosphoric acid, recording mean displacements of 0.320 millimeters versus 0.433 millimeters (p = 0.026). In contrast, posts treated with Er, Cr: YSGG laser irradiation showed no statistically significant difference in displacement between autoclaved and non-autoclaved groups, measuring 0.404 millimeters and 0.358 millimeters, respectively (p = 0.635). The Fisher–Freeman–Halton exact test indicated that failure mode distributions did not differ significantly among the experimental groups (p = 0.674).
The study authors concluded that while autoclave sterilization did not produce significant differences in peak pull-out force, its effect on displacement at maximum force depended on the specific surface treatment applied. The researchers emphasized that these in vitro findings establish neither clinical safety nor therapeutic equivalence, particularly because the experimental sterilization protocol deviates from the post manufacturer instructions.
Subject of Research: Effects of autoclave sterilization and surface treatments on dental fiber post retention
Article Title: Influence of autoclave sterilization on the pull-out characteristics of fiber posts subjected to different surface treatments: an in vitro study
Article References: Sungur Güzel, R., Akbal Dinçer, G., & Sürenler, Z. C. (2026). Influence of autoclave sterilization on the pull-out characteristics of fiber posts subjected to different surface treatments: an in vitro study. BMC Oral Health. https://doi.org/10.1186/s12903-026-10516-x
Image Credits: AI Generated
DOI: 10.1186/s12903-026-10516-x
Keywords: fiber posts, autoclave sterilization, pull-out force, surface conditioning, Er Cr YSGG laser, phosphoric acid, displacement at maximum force, self-adhesive resin cement, premolars, failure mode analysis, dental biomechanics, in vitro study, post retention, root canal treatment, silanization, two-way ANOVA
News Source: Ophelia Keating. (November 28, 2026). Autoclaving Fiber Posts Does Not Alter Maximum Pull-Out Force in Laboratory Study. Scienmag.