Incorporating a defoamer into redispersible polymer powder-modified joint-filling mortar accelerates freeze–thaw deterioration despite producing notable improvements in early volume stability and water absorption. The study demonstrated that favorable pre-freeze property indicators do not necessarily translate into freeze–thaw durability. Redispersible polymer powder and defoamers are widely used to tune the workability and hardened response of cementitious mortars.
The experimental matrix examined a polypropylene-fiber-reinforced joint-filling mortar across several distinct batch configurations, comprising an unmodified reference mixture, a redispersible polymer powder-modified formulation, a defoamer-modified formulation, and a combined polymer-and-defoamer system. A commercial grout was tested alongside these mixtures to serve as an external performance benchmark. The primary experimental comparison focused directly on the contrast between the redispersible polymer powder system and the combined polymer-and-defoamer formulation. Both primary mixtures maintained an identical mixing water content of 280 kg·m⁻³, with the combined system differing solely through the addition of 0.15% defoamer calculated by binder mass.
Initial laboratory evaluations conducted prior to thermal cycling revealed sharp contrasts across physical, transport, and mechanical parameters between the two key formulations. Relative to the mortar containing only the redispersible polymer powder, the combined polymer-and-defoamer mixture reduced water absorption by 46.0% and decreased 28-day drying shrinkage by 50.0%. Furthermore, the incorporation of the defoamer increased the secant modulus by approximately 23%. However, these gains in volume stability and stiffness were accompanied by significant mechanical trade-offs, as flexural strength fell by 28.8% and compressive strength decreased by 25.4%, while transport permeability showed no measurable improvement.
Longitudinal freeze–thaw tracking showed that the initial physical gains of the combined formulation failed to protect the matrix once cycling commenced. The researchers tracked degradation progression by measuring cumulative mass loss and relative dynamic elastic modulus across sequential freeze–thaw cycles.
The accelerated deterioration caused by defoamer addition was further underscored by time-to-failure metrics and post-cycling residual strength tests. The median first observed cycle at which cumulative mass loss reached or exceeded the critical 5% threshold dropped from 50 cycles in the polymer-only formulation down to 15 cycles in the combined formulation. Residual mechanical evaluations were performed on an independent 15-cycle batch. In these tests, post-freeze–thaw compressive strength reached 23.8 MPa for the polymer-modified mortar compared to only 17.2 MPa for the combined mixture, representing a net reduction of 27.7% in residual load-bearing capacity.
The decoupling between early physical metrics and longitudinal durability indicates that conventional pre-freeze assessments provide incomplete projections of service life for modified cementitious materials. Because substantial reductions in water absorption and shrinkage did not avert early frost damage or loss of elastic integrity, the findings demonstrate that initial performance indicators cannot serve as solitary proxies for cold-weather durability. For polypropylene-fiber-reinforced joint-filling mortars and similar polymer-modified systems, the researchers concluded that durability protocols must integrate pre-freeze mechanical and transport data with active deterioration trajectories and post-exposure residual capacity.
The experimental program brought together academic and transportation infrastructure researchers from the Anyang Institute of Technology in Anyang, China, CCCC First Highway Consultants Co., Ltd. in Xi’an, China, and the Shaanxi Provincial Transportation Planning Design and Research Institute Co., Ltd. in Shaanxi, China. The study was received on 28 September 2026 and accepted on 19 October 2026, with correspondence directed to Leilei Han.
Subject of Research: Freeze–thaw durability of polymer- and defoamer-modified joint-filling mortar
Article Title: Decoupled pre-freeze properties and earlier freeze–thaw deterioration in RDP–defoamer-modified joint-filling mortar
Article References: Xiao, W., Wang, X., Qian, C., & Han, L. (2026). Decoupled pre-freeze properties and earlier freeze–thaw deterioration in RDP–defoamer-modified joint-filling mortar. Frontiers in Materials, 13, Article 2012097. https://doi.org/10.3389/fmats.2026.2012097
Image Credits: AI Generated
DOI: 10.3389/fmats.2026.2012097
Keywords: redispersible polymer powder, defoamer, joint-filling mortar, prefabricated pavement bases, polypropylene fibers, freeze-thaw durability, relative dynamic elastic modulus, mass loss, compressive strength, flexural strength, drying shrinkage, water absorption, secant modulus, cementitious mortars, residual mechanical capacity, permeability
News Source: Neil Sanderson. (November 11, 2026). Adding Defoamer Accelerates Freeze-Thaw Deterioration in Polymer-Modified Pavement Joint Mortar. Scienmag.