A synthesized composite photocatalyst pairing bismuth oxyiodide nanosheets with a carbonized iron-based metal-organic framework achieved 99.5 percent degradation of Rhodamine B dye in aqueous solution under visible light emitting diode irradiation. Synthetic organic dyes represent persistent environmental pollutants originating heavily from textile and dyeing effluents, where they deplete dissolved oxygen, obstruct sunlight transmission, and disrupt aquatic ecosystems. Rhodamine B serves as a common recalcitrant model pollutant in catalytic investigations due to its water solubility and stability, while human exposure to the compound is associated with irritation, carcinogenicity, and neurotoxicity. Pristine iron terephthalate metal-organic frameworks, such as MIL-53(Fe), possess three-dimensional structural flexibility and low toxicity but suffer from wide energy band gaps and rapid electron-hole recombination that severely curtail their intrinsic catalytic performance.
To overcome these electronic limitations, researchers fabricated a heterojunction designated as BiOI@C-M53(Fe) using a two-stage synthesis protocol. The base MIL-53(Fe) framework was first produced through a solvothermal reaction combining iron chloride hexahydrate and terephthalic acid in N,N-dimethylformamide at 150 degrees Celsius for 15 hours. The gathered powder underwent drying and was subsequently calcined at 300 degrees Celsius with a ramp rate of 1 degree Celsius per minute for one hour under ambient atmospheric conditions to yield carbonized C-M53(Fe). This thermal processing introduced conductive carbon species that improved electrical conductivity while retaining the underlying metal-organic coordination framework. Bismuth oxyiodide was then grown on the calcined framework at room temperature via co-precipitation using bismuth nitrate pentahydrate in ethylene glycol and potassium iodide in water. Composites were synthesized with varying framework weight ratios of 4, 8, 16, and 24 percent to identify the optimum compositional loading for pollutant decomposition.
Microstructural and morphological characterization confirmed the successful interfacing of both crystalline phases without framework collapse. Field-emission scanning electron microscopy demonstrated that while pristine MIL-53(Fe) formed uniform polyhedral crystals with smooth facets, carbonization roughened the surface and generated a carbonaceous matrix. Pristine bismuth oxyiodide exhibited loosely packed, irregularly arranged nanoplatelets. In the composite containing 4 percent carbonized framework, BiOI nanosheets were uniformly immobilized across the porous carbonaceous scaffold, forming an entwined, threadlike surface topography with accessible surface voids. Energy-dispersive X-ray spectroscopy identified bismuth, carbon, iron, iodine, and oxygen uniformly distributed across the architecture, with bismuth accounting for 71.48 weight percent of the composite surface. Fourier-transform infrared spectroscopy revealed characteristic dicarboxylate linker vibrations at 1503 and 1392 reciprocal centimeters, iron-oxygen coordination bands at 547 reciprocal centimeters, and bismuth-oxygen bending vibrations at 510 reciprocal centimeters. Powder X-ray diffraction patterns verified the coexistence of tetragonal bismuth oxyiodide planes and intact iron framework peaks.
The optical and surface properties of the hybrid material showed distinct alterations that favored visible light harvesting and interfacial reactant contact. Ultraviolet-visible diffuse reflectance spectroscopy indicated that the absorption edge shifted from approximately 650 nanometers in pure bismuth oxyiodide to 680 nanometers in the composite. Tauc plot extrapolations yielded optical band gap energies of 1.94 electron volts for the carbonized framework, 1.90 electron volts for pure bismuth oxyiodide, and 1.88 electron volts for the 4 percent composite. Brunauer-Emmett-Teller measurements showed surface areas of 2.39 square meters per gram for pure bismuth oxyiodide, 11.39 for pristine MIL-53(Fe), 18.32 for the carbonized framework, and 12.96 for the 4 percent composite. The surface area reduction in the composite relative to the carbonized precursor reflected pore coverage by bismuth oxyiodide nanoplatelets. Photoluminescence analysis using 260 nanometer excitation showed a notable drop in emission intensity at 521 nanometers for the composite, indicating suppressed electron-hole recombination. Furthermore, zeta potential measurements yielded a value of positive 60.5 millivolts, providing strong electrostatic dispersion stability.
Photocatalytic evaluation established that the 4 percent composite surpassed all individual components and alternative mass loadings under visible light emitting diode exposure delivering 98,000 lux. Under benchmark conditions with 10 milligrams per liter Rhodamine B, pristine MIL-53(Fe) at a concentration of 0.5 grams per liter removed only 7.6 percent of the dye after 120 minutes, primarily via surface adsorption due to poor visible absorbance. Unmodified bismuth oxyiodide removed 29 percent and the carbonized framework removed 35 percent over the same period. Among composite formulations, activity ranked in the order of 4 percent, 16 percent, 8 percent, and 24 percent, demonstrating that catalytic efficiency did not follow a linear relationship with framework loading. Photolysis tests without any catalyst produced less than 1 percent dye loss. Ultraviolet-visible absorption profiles recorded at progressive intervals showed that the primary dye absorption peak at 553 nanometers steadily declined and approached zero after 120 minutes, confirming that contaminant disappearance was driven by catalytic cleavage rather than phase partitioning alone.
Operating parameters were systematically optimized using a three-factor, three-level Box-Behnken experimental design comprising 17 runs. The three evaluated independent variables were solution pH ranging from 4 to 10, catalyst dose from 0.2 to 1.0 grams per liter, and irradiation time from 30 to 120 minutes. Analysis of variance yielded a second-order polynomial quadratic regression model with an F-value of 70.98 and a p-value below 0.0001, demonstrating high statistical significance. The coefficient of determination reached 0.98, the adjusted R-squared was 0.96, and the predicted R-squared was 0.89, while the lack-of-fit test showed an F-value of 1.63 with a p-value of 0.33, confirming model validity. Catalyst dose exhibited the largest positive coefficient, establishing it as the most influential factor. Conversely, increasing solution pH produced a negative effect on degradation. Numerical solving of the model predicted optimal removal at pH 5.6, a catalyst dosage of 1.0 gram per liter, and an irradiation duration of 113 minutes, forecasting 99.7 percent efficiency. Laboratory verification under these parameters in triplicate achieved an average degradation of 99.5 percent.
Experimental data were fitted against non-linear pseudo-first-order and pseudo-second-order kinetic expressions across initial dye concentrations of 5, 10, and 15 milligrams per liter. Under visible light emitting diode illumination, the pseudo-second-order model yielded lower residual sum of squares and reduced chi-square values across all tested concentrations, producing an apparent rate constant of 0.04 liters per milligram per minute at 10 milligrams per liter. Under natural solar irradiation, complete dye clearance occurred within rapid timescales, reaching 100 percent removal for 10 milligrams per liter. However, neither kinetic model consistently outperformed the other under solar conditions: the pseudo-first-order formulation showed superior fit at 10 milligrams per liter with an apparent rate constant of 0.18 reciprocal minutes, while the pseudo-second-order model yielded a slightly better statistical fit at 15 milligrams per liter.
Mechanistic pathways and active oxidative species were investigated through scavenger trapping experiments and semiconductor band structure determinations. The introduction of 10 millimolar concentrations of isopropyl alcohol for hydroxyl radicals, potassium iodide for photogenerated holes, and silver nitrate for conduction band electrons produced only minor impacts on reaction rates. In contrast, benzoquinone, which selectively captures superoxide radicals, caused dye degradation to decrease from 99.8 percent down to 63.2 percent, highlighting the dominant role of oxygen-derived radical species. Mott-Schottky measurements exhibited positive slopes confirming n-type semiconductor behavior for both materials, showing flat-band potentials of negative 0.22 volts for bismuth oxyiodide and positive 0.42 volts for the carbonized framework versus silver/silver chloride electrodes. Conduction band edges were calculated at negative 0.20 volts and positive 0.44 volts versus the normal hydrogen electrode, with corresponding valence band edges at positive 1.66 volts and positive 2.38 volts. Because the conduction band of bismuth oxyiodide is insufficient to drive unassisted direct reduction of dissolved oxygen, the authors proposed that interfacial electron migration between phases and iron redox cycling facilitate the generation of reactive oxygen intermediates.
Practical treatment feasibility was scrutinized through mineralization analysis, real-water matrix trials, recycling stability assessments, and multi-dye tests. Chemical oxygen demand measurements revealed a 79.5 percent reduction from an initial 79.7 milligrams per liter to 16.3 milligrams per liter after 113 minutes of treatment. While substantial, this value was lower than the 99.7 percent decolorization efficiency, indicating that intermediate organic fragments persisted in solution following chromophore breakdown. When tested in a natural water matrix containing competing ionic species including calcium, magnesium, sodium, chloride, and nitrate, Rhodamine B degradation was noticeably attenuated compared to synthetic solutions. Catalyst reusability tests showed an efficiency decline of approximately 40 percent across four successive cycles, which post-reaction diffraction and infrared characterization attributed to active site blockage by adsorbed byproducts and minor metal dissolution rather than crystallographic collapse. Inductively coupled plasma spectrometry confirmed aqueous leaching concentrations of 0.159 milligrams per liter for iron and 2.59 milligrams per liter for bismuth under optimal operating conditions, remaining below pertinent drinking water thresholds.
Biological and ecological safety assessments demonstrated that the photocatalytic breakdown process markedly lowered solution toxicity. In phytotoxicity assays conducted on watercress seeds over three days of incubation at 30 degrees Celsius, untreated 10 milligram per liter dye solutions suppressed seed performance, yielding a germination index of 45.9 percent and an average root length of 1.7 centimeters. Following photocatalytic treatment with the composite, seed germination indices and root elongation recovered to levels virtually identical to distilled water controls. Parallel ecotoxicity evaluations utilizing bioluminescent Vibrio harveyi bacteria demonstrated that the inhibition of light emission decreased following catalytic treatment, corroborating the mitigation of environmental toxicity. Broad-spectrum evaluations against distinct dye classes revealed preferred degradation performance toward anionic dyes, reaching 97 percent removal for Carmoisine and 77 percent for Eriochrome Black T, compared to 25 percent for Malachite Green and 23 percent for Methylene Blue, underscoring the influence of surface electrostatic interactions on catalytic breakdown.
Subject of Research: Photocatalytic degradation of Rhodamine B using a BiOI and carbonized MIL-53(Fe) heterojunction catalyst
Article Title: MOF-derived heterojunction for energy-efficient degradation of Rhodamine B; LED and solar irradiation, mechanism, and toxicity insights
Article References: Nabavi, B. F., Alidadi, H., Kh. Abdalameer, N., Shams, M., & Barghi, A. (2026). MOF-derived heterojunction for energy-efficient degradation of Rhodamine B; LED and solar irradiation, mechanism, and toxicity insights. Results in Engineering, 32, Article 113972. https://doi.org/10.1016/j.rineng.2026.113972
Image Credits: AI Generated
DOI: 10.1016/j.rineng.2026.113972
Keywords: BiOI, MIL-53(Fe), photocatalysis, heterojunction, Rhodamine B, water treatment, Box-Behnken design, visible light degradation, chemical oxygen demand, superoxide radicals, phytotoxicity, Vibrio harveyi, metal leaching, calcined MOF, organic dye removal, reaction kinetics, semiconductor band gap
News Source: Denise Maddox. (November 12, 2026). Bismuth Oxyiodide Framework Heterojunction Degrades Rhodamine B Under Visible Light. Scienmag.