Pb-Sn alloy reaches 10,180% superplastic elongation after tube high-pressure shearing
An experimental study reported 10,180% superplastic elongation in a hypoeutectic Pb-40 wt% Sn alloy processed by tube high-pressure shearing.
An experimental study reported 10,180% superplastic elongation in a hypoeutectic Pb-40 wt% Sn alloy processed by tube high-pressure shearing.
Compression tests of an as-cast nitrogen-containing Fe–Mn–Co–Cr high-entropy alloy reveal that dynamic recovery, continuous recrystallization and grain refinement shift substantially ...
A laboratory casting study found that CuO nanoparticles refined A356 alloy grains and modified eutectic silicon while increasing microhardness, reducing ...
Researchers show that a 10 Hz alternating magnetic field during melt treatment disperses ZrB2 and Al2O3 nanoparticles most uniformly in ...
Researchers used room-temperature surface mechanical attrition treatment to refine the grains of Inconel X-750, raising surface hardness by 12.5 percent ...
Adding zirconium oxide to yttria-strengthened tungsten refines grains and boosts compressive strength by up to 44 percent at room temperature ...
Researchers show that adjusting extrusion temperature between 280 and 360 degrees Celsius tunes the strength, ductility, corrosion resistance and thermal ...
New microscopic research reveals how grain refinement and grain boundary precipitates slow hydrogen diffusion in austenitic stainless steels, offering a ...
Researchers report that adding trace aluminum, manganese and copper to a high-magnesium zinc alloy produces a homogeneous fine-grained microstructure that ...
Researchers in China show that a moderate rolling speed of 1024 mm/s gives a biodegradable Mg–2Zn–0.4Ca alloy its finest grains, ...
Researchers at AGH University of Krakow used cyclic extrusion–compression to tune the microstructure of biodegradable zinc–magnesium alloys, achieving an enhanced ...
New research shows that rolling 9Cr-ODS steel within the intercritical temperature window preserves its strengthening nano-oxides and delivers higher strength ...
Researchers at Jilin University report that micro-scale copper and nano-scale silicon carbide particles, combined through ball milling and friction stir ...
Researchers report that tuning scandium content between 0.16 and 0.50 percent in wire arc additive manufactured Al-Mg-Sc alloys refines grains ...
Adding 1.5 weight percent iron to 3D-printed Ti5553 titanium alloy nearly halves its columnar grain width and boosts strength to ...
Researchers report that nickel composites reinforced with hybrid micro- and nanosized silicon carbide particles reached 1526 MPa tensile strength and ...
Adding as little as 0.05 to 0.1 weight percent titanium nanoparticles during wire arc additive manufacturing refines the coarse grains ...