Friction Stir Deposition Refines 1018 Carbon Steel Grains and Enhances Wear Resistance
Additive friction stir deposition achieved approximately 60 percent grain refinement and reduced wear rates in 1018 carbon steel despite accelerating ...
Additive friction stir deposition achieved approximately 60 percent grain refinement and reduced wear rates in 1018 carbon steel despite accelerating ...
A combined transmission electron microscopy and atomistic simulation study reveals that cryogenic deformation at 83 Kelvin lowers stacking fault energy ...
Increasing manganese content from 0.11 to 0.49 weight percent in Al–Mg–Si-based alloys altered the size and density of dispersoids while ...
Hot-compression tests demonstrate that squeeze-cast AA7075 alloy preforms achieve enhanced forgeability through dynamic recrystallization and optimized power dissipation domains.
An experimental compression study reports how temperature, strain rate and loading history affected flow stress, texture and continuous dynamic recrystallization ...
Compression tests of an as-cast nitrogen-containing Fe–Mn–Co–Cr high-entropy alloy reveal that dynamic recovery, continuous recrystallization and grain refinement shift substantially ...
A harmonic-structured CoCrFeMnNi high-entropy alloy shows pronounced flow softening at high temperatures because its ultrafine-grained shell network recovers preferentially while ...