Researchers evaluating resin-based dental restoratives produced by additive and subtractive manufacturing have found that surface properties change significantly when materials are subjected to simulated thermal aging. Across the tested specimens, thermal cycling increased overall surface roughness, while the effect of surface treatments on color stability varied depending on the specific resin composition.
The laboratory investigation examined how different fabrication workflows and finishing techniques withstand environmental conditions designed to mimic the thermal stress of the human mouth. To assess these behaviors, the study evaluated eighty disc-shaped dental specimens, each prepared in an A2 shade with standardized dimensions of ten millimeters in diameter and two millimeters in thickness.
Specimen production encompassed four distinct material systems, consisting of one subtractive computer-aided design and manufacturing resin block, Voco Grandio Disc, alongside three additive resins formulated for three-dimensional printing: Bego VarseoSmile TriniQ, Saremco Print Crowntec, and NextDent C&B MFH. Following fabrication, each specimen was assigned to receive either conventional mechanical polishing or a protective surface sealant application using Optiglaze.
To evaluate post-treatment stability under intraoral conditions, all eighty prepared discs underwent five thousand thermal aging cycles alternating between water baths set at five degrees Celsius and fifty-five degrees Celsius. Color variations were quantified using a digital spectrophotometer to calculate color difference values, while contact profilometry recorded changes in surface roughness before and after thermal stress.
Statistical evaluation revealed a significant interaction between restorative material type and surface treatment for overall color stability. Notably, applying a surface sealant produced a statistically significant difference in color stability compared to mechanical polishing exclusively within the NextDent group, whereas differences in other material groups did not reach that threshold.
Thermal aging exerted a statistically significant main effect across the test groups by increasing overall surface roughness values. The overall three-way interaction between material formulation, surface treatment method, and thermal aging was not statistically significant, though exploratory post hoc testing suggested an isolated roughness increase in sealant-treated TriniQ specimens that warrants cautious interpretation.
The study demonstrated that finishing protocols and restorative compositions directly govern the physical response of printed and milled dental polymers to thermal cycling. Selecting specific surface finishing protocols aligned with material composition remains essential for optimizing the long-term surface integrity of resin-based dental restorations.
To evaluate the experimental data rigorously, the researchers implemented two way analysis of variance alongside repeated measures analysis of variance, establishing their formal significance threshold at an alpha value of zero point zero five. This analytical structure enabled the investigators to verify whether color stability shifts and surface roughness changes stemmed from specific materials, surface sealants, or aging.
The computations confirmed that thermal aging increased overall roughness with a probability value of zero point zero one six. Additionally, the interactive effect on color difference yielded a value below zero point zero zero one, whereas the three way interaction produced zero point three four seven, meaning the exploratory increase yielding zero point zero three nine warrants caution.
Subject of Research: Color stability and surface roughness of manufactured resin-based dental restorative materials following thermal aging
Article Title: Evaluation of color stability and surface roughness of resin-based restorative materials produced with additive and subtractive manufacturing technologies after thermal aging
Article References: Yaprak Kirbiyik, A., Guleryuz, A., Erbas, T., & Ekici, B. (2026). Evaluation of color stability and surface roughness of resin-based restorative materials produced with additive and subtractive manufacturing technologies after thermal aging. BMC Oral Health. https://doi.org/10.1186/s12903-026-10431-1
Image Credits: AI Generated
DOI: 10.1186/s12903-026-10431-1
Keywords: dental materials, resin-based restoratives, additive manufacturing, subtractive manufacturing, thermal aging, surface roughness, color stability, spectrophotometry, profilometry, Optiglaze, mechanical polishing, Voco Grandio Disc, Bego VarseoSmile TriniQ, Saremco Print Crowntec, NextDent, dental 3D printing, biomaterials, thermal stress
News Source: Beatrice Stafford. (November 28, 2026). Thermal Aging Increases Surface Roughness in Resin-Based Dental Restorative Materials. Scienmag.