Materials scientists have demonstrated that altering the scanning trajectory of an ultrasonically excited pulsating water jet directly controls the surface texture, directional uniformity, and subsurface hardness of AISI 316 L stainless steel without introducing solid abrasives or heat. In an experimental investigation published in Archives of Civil and Mechanical Engineering, researchers evaluated how high-frequency clusters of water droplets modify metallic workpieces when guided along either a single-direction linear path or a perpendicular crisscross path. The findings confirm that while conventional abrasive water jets can leave contaminating particles embedded in treated workpieces, an acoustic field can instead modulate continuous water streams into high-energy droplet impacts that overcome the metal yield point at moderate supply pressures. Changing the path taken across the steel surface fundamentally dictates whether the resulting topography is deeply pitted and directional or comparatively smooth and directionally uniform, establishing droplet distribution as a precise parameter for surface functionalization.
Conventional mechanical and thermal surface treatments, including shot peening, grinding, laser processing, and chemical nitriding, are widely employed to improve fatigue, wear, and corrosion resistance across aerospace, automotive, energy, and biomedical components. However, these traditional processes frequently produce heat-affected zones, unwanted residual stress states, or environmental contamination. While abrasive water jet technology avoids heat generation and provides omnidirectional cutting of high-strength alloys and ceramics, the continuous consumption of solid abrasives introduces substantial operating expenses, nozzle wear, and the persistent hazard of abrasive particles embedding themselves directly into the component. To overcome these limitations, researchers have focused on abrasive-less water jets. The ultrasonic pulsating water jet relies on a piezoelectric transducer attached to an ultrasonic sonotrode within an acoustic chamber, operating at an excitation frequency of approximately 20 kHz. This setup induces rapid pressure fluctuations and acoustic cavitation within the pressurized water column, transforming the outflow into a train of discrete droplet clusters that generate intense localized impact pressures, lateral jetting, and cavitation collapse upon reaching the target.
Despite the known physics of isolated droplet collisions, previous investigations into pulsating water jets largely concentrated on localized erosion pits or basic linear scanning paths at low operating pressures, leaving a significant gap in understanding how wide-area scanning trajectories govern cumulative surface changes. The research team examined this synergy by designing an experimental framework using hot-rolled AISI 316 L austenitic stainless steel blocks measuring 90 by 25 by 20 millimeters. Austenitic stainless steel was selected for its homogeneous non-magnetic microstructure, moderate toughness, and established corrosion resistance, ensuring that post-treatment morphological transformations could be attributed entirely to mechanical impact rather than chemical corrosion artifacts. Before exposure, the block specimens were ground metallographically to a P2500 mesh finish, yielding a baseline arithmetic mean surface roughness of Sa = 0.03 micrometers, a maximum height Sz of 0.4131 micrometers, and an initial isotropy of only 1.59 percent due to prominent, parallel grind marks.
The experimental setup utilized an acoustic chamber length of 22 millimeters and positioned the jet at an optimal standoff distance of 116 millimeters above the workpiece, delivering water at a controlled supply pressure and flow rate to treat square target areas measuring 20 by 20 millimeters. To achieve consistent areal coverage, the step-over distance between adjacent passes was set to 0.55 millimeters, representing an overlapping factor of 25 percent of the 2.2-millimeter erosion footprint. The team systematically contrasted two specific exposure paths: a one-directional Linear strategy executed at a traverse speed of 6 millimeters per second, and a two-pass CrissCross strategy where an initial pass was followed by a perpendicular second run at 12 millimeters per second. Because the CrissCross strategy doubled the traverse speed across its two orthogonal stages, both processing routines maintained an identical total exposure time and the exact same number of droplet impacts per unit length, isolating the physical influence of scanning geometry from the total delivered energy.
Topographical evaluations conducted across the treated regions using coherence scanning interferometry revealed striking differences in surface roughness between the two distribution strategies. The Linear scanning path increased the arithmetic mean height from the untreated baseline of 0.03 micrometers up to 7.5 micrometers, whereas the orthogonal CrissCross trajectory produced a significantly more moderate increase to 3.5 micrometers. Similarly, maximum height Sz expanded from 0.4131 micrometers on the ground surface to 107 micrometers under the Linear trajectory, compared to 76 micrometers for the CrissCross path. The researchers determined that the Linear approach concentrates repetitive droplet collisions and unilateral lateral jetting along a single axis, digging deeper microcraters and throwing up substantial plastic ridges. In contrast, the second orthogonal run of the CrissCross pattern cuts across the initial deformation tracks at higher velocity, partially eroding and redistributing elevated peak features into a more balanced areal profile.
This selective peak-damping effect was further corroborated by analyzing the peak height Sp and pit depth Sv parameters. On the untreated steel, Sp and Sv measured 0.1943 micrometers and 0.2188 micrometers, respectively. Following pulsating jet peening, peak height Sp reached approximately 52 micrometers under the Linear strategy but remained constrained to roughly 30 micrometers under the CrissCross routine, while pit depth Sv reached roughly 55 micrometers for Linear and 45 micrometers for CrissCross. The pronounced disparity in peak reduction indicates that while the perpendicular pass effectively shears away or flattens tall uplifted rims, the deep crater-like valleys created during early impacts remain largely sheltered. Consequently, the CrissCross strategy preserves internal retention volume while avoiding extreme peak projections, an advantageous profile for tribological contacts and sealing surfaces where elevated asperity contacts must be minimized without losing fluid reservoirs.
Statistical height distribution metrics confirmed that both jet strategies transitioned the original symmetric Gaussian profile into a distinctly valley-dominated landscape. The untreated ground steel exhibited a skewness Ssk of 0.031 and a kurtosis Sku of 3.057. Following treatment, skewness shifted into negative values, dropping to approximately minus 0.75 for the Linear trajectory and minus 0.35 for the CrissCross trajectory, demonstrating that both finished profiles feature plateau-like surfaces dominated by deep recessions rather than sharp projections. Kurtosis rose to roughly 4.8 under the Linear path and 5.6 under the CrissCross path, showing that the remaining microtopography consists of leptokurtic, localized extremes formed by discrete droplet impacts rather than normal random roughness. Simultaneously, the developed interfacial area ratio Sdr surged from 0.006 percent on the ground baseline to 64 percent for the Linear trajectory and 34 percent for the CrissCross path, while surface isotropy climbed from 1.59 percent to approximately 88 percent and 93 percent, respectively, demonstrating that multi-directional scanning almost entirely erases prior grinding marks.
Detailed scanning electron microscopy accompanied by optical microscopy revealed the specific micromechanical deformation mechanisms responsible for these macroscopic roughness variations. At low magnification, optical imaging showed that the CrissCross trajectory produced a visually homogeneous field free of distinct waviness, whereas higher-magnification scanning electron micrographs showed connected microcracks, erosion craters, and uplifted metallic ridges driven by lateral fluid outflow. High-speed lateral jetting impacts existing surface irregularities, driving local shear deformation and creating undercut cavities beneath the observable plane. In the transitional boundary zones bordering the untreated metal, the Linear trajectory exhibited visible disparities in local erosion depth, whereas the rolling-over effect of the second perpendicular pass in the CrissCross path smoothed out the transitional perimeter. High-magnification fractography at 10,000 times magnification confirmed that damage frequently initiated along legacy grinding grooves and grain boundaries, where stress concentrations accelerate crack propagation and localized plastic displacement.
Subsurface mechanical assessments demonstrated that pulsating water jet peening imparts substantial work hardening beneath the eroded topography. Cross-sectional microhardness maps acquired using an instrumented testing system with a 15-gram load starting at a depth of 30 micrometers revealed a work-hardened zone extending 150 to 200 micrometers into the bulk alloy. At the initial 30-micrometer measurement depth, microhardness increased by 18 percent to 368.60 HV0.015 for the Linear strategy and by 17.3 percent to 366.41 HV0.015 for the CrissCross strategy, compared to 312.58 HV0.015 for the untreated metal. Top-surface Vickers HV5 testing showed slightly higher overall values for the Linear path but exhibited measurement artifacts due to surface roughness and indenter contact geometry. Electron backscatter diffraction analysis linked this subsurface hardening to intense plastic strain, an accumulation of dislocation density, deformation twinning, and the subsequent generation of low-angle grain boundaries within the original austenitic grains.
Contact angle and surface free energy measurements conducted after one month of ambient laboratory storage demonstrated that the mechanical treatment also modifies surface wetting behavior in a selective manner. Testing with deionized water showed that the apparent contact angle increased from 69.41 degrees on the hydrophilic ground surface to 93.59 degrees for the Linear path and 91.87 degrees for the CrissCross path, reflecting incomplete wetting and air entrapment within deep microscopic asperities consistent with Cassie-Baxter mechanics. Conversely, testing with non-polar alpha-bromonaphthalene saw contact angles drop sharply from an initial 26.95 degrees down to 12.40 degrees for the Linear trajectory and 9.60 degrees for the CrissCross trajectory. Surface free energy calculations using the Owens-Wendt model revealed that peening nearly eliminated the polar surface energy component, dropping it from 7.6 millinewtons per meter to 0.2 and 0.4 millinewtons per meter, while increasing the dispersive component from 39.7 millinewtons per meter to 43.4 and 43.8 millinewtons per meter.
The study authors emphasized several analytical limitations, noting that residual stresses were not directly measured, leaving their precise role in near-surface stress states unquantified. Furthermore, because contact angles were evaluated after extended ambient storage rather than immediately after processing, and without direct spectroscopic chemical analysis such as X-ray photoelectron spectroscopy, the wetting shift represents a combined consequence of altered topography and ambient atmospheric aging, including potential passive-film rearrangement and hydrocarbon adsorption. Future work must incorporate time-resolved wetting measurements, residual stress profiling, and systematic tribological and corrosion evaluations. Nevertheless, the experimental evidence establishes that by selecting between linear and orthogonal scanning paths, engineers can tailor pulsating water jet peening to produce either aggressive mechanical interlocking textures or directionally uniform, isotropic functional surfaces on stainless steel without chemical or thermal side effects.
Subject of Research: Surface functionalization of AISI 316 L stainless steel using ultrasonic pulsating water jet peening
Article Title: Influence of droplet distribution strategy on surface functionalization of stainless steel 316 L by ultrasonically excited pulsating water jet peening
Article References: Nag, A., Chlupová, A., Gupta, M. K., Poloprudský, J., Stolarik, G., Sobola, D., Šiška, F., Nieslony, P., & Hloch, S. (2026). Influence of droplet distribution strategy on surface functionalization of stainless steel 316 L by ultrasonically excited pulsating water jet peening. Archives of Civil and Mechanical Engineering, 26(6), Article 278. https://doi.org/10.1007/s43452-026-01643-x
Image Credits: AI Generated
DOI: 10.1007/s43452-026-01643-x
Keywords: Pulsating water jet, Water jet peening, AISI 316 L stainless steel, Surface topography, Surface functionalization, Scanning trajectory, CrissCross scanning, Areal surface roughness, Subsurface microhardness, Work hardening, Selective wettability, Contact angle, Surface free energy, Abrasive-less machining, Ultrasonic sonotrode, Dispersive surface energy, Plastic deformation
News Source: Denise Maddox. (November 23, 2026). Pulsating Water Jets Modify Stainless Steel Texture Based on Droplet Trajectory. Scienmag.